$86.00 Original price was: $86.00.$49.02Current price is: $49.02.
Heat Up Time(STABILIZED May 2012)
Category: AIR
Tags: Copper, Engine cylinders, Gases, Heat transfer, Heat treatment, Metals, Plating, Steel, Titanium
Description
An analysis was made of the effects of various surface conditions on the heat up time of steel bars which are heated in atmosphere furnaces to the temperature range used for steel hardening or normalizing. The purpose was to examine whether a standard heating time for a given section thickness is acceptable.
History
| AIR4279A | 2012-05-09 | Latest | Stabilized |
| AIR4279 | 1995-05-01 | Historical | Issued |
| ISSUING COMMITTEE | AMS AMEC Aerospace Metals and Engineering Committee |
|---|---|
| DATE | 2012-05-09 |
| DOI | |
| ISCURRENT | Current |
| PAGE | 8 |
| PUBLISHER | SAE International |
| REVISED | STABILIZED |