SAE AMS4144G PDF
$91.00 Original price was: $91.00.$51.87Current price is: $51.87.
Aluminum Alloy, Hand Forgings and Rolled Rings 6.3Cu – 0.30Mn – 0.18Zr – 0.10V – 0.06Ti (2219-T852/T851) Solution Heat Treated, Mechanically Stress Relieved, and Precipitation Heat Treated
Category: AMS
Tags: Aluminum, Aluminum alloys, Heat treatment, Magnesium, Magnesium alloys, Materials properties, Metals, Non-destructive tests, Tensile strength
Description
This specification covers an aluminum alloy in the form of hand forgings 17 inches (432 mm) and under in nominal thickness, and rolled rings up to 6 inches, incl (152 mm, incl) in nominal thickness at the time of heat treatment (see 8.5).
History
| AMS4144H | 2025-02-25 | Latest | Revised |
| AMS4144G | 2020-02-18 | Historical | Revised |
| AMS4144F | 2011-09-28 | Historical | Reaffirmed |
| AMS4144E | 1995-07-01 | Historical | Revised |
| AMS4144D | 1991-07-01 | Historical | Revised |
| AMS4144C | 1985-07-01 | Historical | Revised |
| AMS4144B | 1979-10-01 | Historical | Revised |
| AMS4144A | 1975-06-01 | Historical | Revised |
| AMS4144 | 1965-09-01 | Historical | Issued |
| ISSUING COMMITTEE | AMS D Nonferrous Alloys Committee |
|---|---|
| DATE | 2020-02-18 |
| DOI | |
| ISCURRENT | |
| PAGE | 9 |
| PUBLISHER | SAE International |
| REVISED | REVISED |