ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base – 19Cr – 3.1Mo – 5.1(Cb + Ta) – 0.90Ti – 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated
Description
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base – 19Cr – 3.1Mo – 5.1(Cb + Ta) – 0.90Ti – 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated
History
| AMS5664G | 2022-08-17 | Latest | Revised |
| AMS5664F | 2017-01-03 | Historical | Revised |
| AMS5664E | 2006-04-19 | Historical | Reaffirmed |
| AMS5664D | 1994-07-01 | Historical | Revised |
| AMS5664C | 1990-10-01 | Historical | Revised |
| AMS5664B | 1980-10-01 | Historical | Revised |
| AMS5664A | 1967-11-01 | Historical | Revised |
| AMS5664 | 1965-09-01 | Historical | Issued |
| ISSUING COMMITTEE | AMS F Corrosion and Heat Resistant Alloys Committee |
|---|---|
| DATE | 1967-11-01 |
| DOI | |
| ISCURRENT | |
| PAGE | 3 |
| PUBLISHER | SAE International |
| REVISED | REVISED |
Please select a variation to view its pdf.






Reviews
There are no reviews yet.