SAE AMS5919C PDF

Original price was: $75.00.Current price is: $42.75.

Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Round Bars 19Cr – 36Co – 25Ni – 7.0Mo – 0.50Cb (Nb) – 2.9Ti – 0.20Al – 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened, Modified Strength

PDF Format Searchable Printable Bookmarks
Guaranteed Safe Checkout

Description

This specification covers a corrosion- and heat-resistant, work strengthened cobalt-nickel-chromium alloy in the form of bars 2 inches (50 mm) and under in nominal diameter).

History

AMS5919C 2024-06-26 Latest Revised
AMS5919B 2018-08-08 Historical Revised
AMS5919A 2013-02-07 Historical Revised
AMS5919 2007-08-24 Historical Reaffirmed
ISSUING COMMITTEE

AMS F Corrosion and Heat Resistant Alloys Committee

DATE

2024-06-26

DOI

https://doi.org/10.4271/AMS5919C

ISCURRENT

Current

PAGE

6

PUBLISHER

SAE International

REVISED

REVISED

Reviews

There are no reviews yet.

Be the first to review “SAE AMS5919C PDF”

Your email address will not be published. Required fields are marked *

Please select a variation to view its pdf.

SAE AMS5919C PDF
$75.00 Original price was: $75.00.$42.75Current price is: $42.75.